Product Parameters
| 
				 Product Specification 
					  Specification 
					    | 
		|||||||||||||||
| 
				Property | 
			
				Test Method | 
			
				Unit | 
			
				Test data | 
		||||||||||||
| Tensile Strength | 
				ISO527 | 
			
				MPa | 
			
				22.6 | 
		||||||||||||
| Tear Trength | 
				ISO527 | 
			
				MPa | 
			20.1 | ||||||||||||
| Proportion | 
				ISO1183 | 
			
				g/cm3 | 
			
				 1.05 | 
		||||||||||||
| UV Resistance | 
				UVA  315-400nm  | 
			
				240H | 
			
				UVA Treated  OK  | 
		||||||||||||
| 
				High and low temperature test | 
			
				GB/T  2423.1-2001  | 
			
				100 cycles | 
			
				Qualified OK (-30℃-+80℃)  | 
		||||||||||||
| 
				Vicat  Softening Temperature  | 
			
				ISO306 | 
			
				℃ | 
			
				77.9 | 
		||||||||||||
| Heat Distortion Temp | 
				ISO75 | 
			
				℃ | 
			
				93.8 | 
		||||||||||||
| Fire rating | 
				UL94 | 
			
				class | 
			
				V2 | 
		||||||||||||
| Transmittance | 
				GB2410-80 | 
			
				% | 
			
				61.2 | 
		||||||||||||
| Haze | 
				GB2410-80 | 
			
				% | 
			
				91.7 | 
		||||||||||||
| RoHS | 
				Directive  2011/65/EU (RoHs)  | 
			
				— — | 
			
				Pass | 
		||||||||||||
| SVHC | 
				Regulation (EC)  No 1907/2006 (REACH)  | 
			
				— — | 
			
				Pass | 
		||||||||||||
| GWEPT | 
				IEC  60695-2-11:2021  | 
			
				℃ | 
			
				750 | 
		||||||||||||
| 
				 | 
			
				 | 
			
				 | 
			
				 | 
		||||||||||||
	
	
	
	Product Utilization

The product uses nano-modification technology to change the molecular structure of PP and add nano-sized light diffuser agents, transforming point or line light source into soft and uniform surface light source. Nano PP material has good environmental performance, high resilience, strong yellowing resistance and flame retardant V2 rating.  
	
 
	